ELABORATION ET ETUDE DE LA TENUE A L'OXYDATION A HAUTE TEMPERATURE D'ALLIAGES DE SURFACE OBTENUS PAR IRRADIATION LASER SUR DEUX ACIERS FERRITIQUES PEU ALLIES

ELABORATION ET ETUDE DE LA TENUE A L'OXYDATION A HAUTE TEMPERATURE D'ALLIAGES DE SURFACE OBTENUS PAR IRRADIATION LASER SUR DEUX ACIERS FERRITIQUES PEU ALLIES PDF Author: ENORI.. GEMELLI
Publisher:
ISBN:
Category :
Languages : fr
Pages : 159

Get Book Here

Book Description
L'OBJECTIF DU TRAVAIL PRESENTE ICI EST D'AUGMENTER, PAR UN TRAITEMENT DE SURFACE, LA TENUE A L'OXYDATION A TEMPERATURE ELEVEE ET LA DURETE D'ACIERS FERRITIQUES FAIBLEMENT ALLIES. NOUS PRESENTONS LES RESULTATS OBTENUS AVEC LES ACIERS 35NCD16 ET Z38CDV5 PAR IRRADIATION LASER ASSURANT L'INCORPORATION SUPERFICIELLE ET LA DISSOLUTION DE PREDEPOTS DE NITRURES (ALN, SI#3N#4) OU DE CARBURES (SIC, CR#3C#2). NOUS PRECISIONS LES CONDITIONS D'OBTENTION D'ALLIAGES DE SURFACE EXEMPTS DE FISSURES, D'AMAS OU DE POROSITES. LA DURETE DE CES ALLIAGES DEPEND PRINCIPALEMENT DE LA FORMATION DE MARTENSITE ET (OU) DE LA PRECIPITATION DE CARBURES OU DE NITRURES. L'EXCELLENTE TENUE A L'OXYDATION EN CONDITIONS ISOTHERMES JUSQU'A 950C DE QUELQUES ALLIAGES DE SURFACE DANS UNE ATMOSPHERE D'OXYGENE RESULTE ESSENTIELLEMENT DE LA FORMATION D'UNE COUCHE D'OXYDE DE CHROME CR#2O#3. DANS LES ALLIAGES CONTENANT DU SILICIUM ET RELATIVEMENT PEU DE CHROME, LA CROISSANCE DE CETTE COUCHE DE CR#2O#3 N'INTERVIENT QU'APRES CELLE, INITIALE, D'UNE TRES MINCE PELLICULE DE SILICE QUI INHIBE L'OXYDATION DU FER ET REND POSSIBLE LE DEVELOPPEMENT DE LA COUCHE PROTECTRICE DE CR#2O#3. LE BON COMPORTEMENT EN CYCLAGE THERMIQUE DES ALLIAGES DE SURFACE ETUDIEES SUR L'ACIER Z38CDV5 RESULTERAIT DE LA CROISSANCE DE CR#2O#3 PAR DIFFUSION ANIONIQUE. LA PETITE TAILLE DE GRAINS DE CET OXYDE PERMETTRAIT UNE BONNE RELAXATION DE CONTRAINTES THERMIQUES PAR DEFORMATION PLASTIQUE. NOUS AVONS DONC MONTRE QUE LE TRAITEMENT LASER AVEC AJOUT PEUT CONSTITUER UN PROCEDE EFFICACE POUR CONFERER AUX ACIERS PEU ALLIES UN COMPORTEMENT EN OXYDATION A HAUTE TEMPERATURE TOUT A FAIT COMPARABLE A CELUI DES ACIERS INOXYDABLES AVEC L'AVANTAGE D'UNE DURETE PLUS ELEVEE

ELABORATION ET ETUDE DE LA TENUE A L'OXYDATION A HAUTE TEMPERATURE D'ALLIAGES DE SURFACE OBTENUS PAR IRRADIATION LASER SUR DEUX ACIERS FERRITIQUES PEU ALLIES

ELABORATION ET ETUDE DE LA TENUE A L'OXYDATION A HAUTE TEMPERATURE D'ALLIAGES DE SURFACE OBTENUS PAR IRRADIATION LASER SUR DEUX ACIERS FERRITIQUES PEU ALLIES PDF Author: ENORI.. GEMELLI
Publisher:
ISBN:
Category :
Languages : fr
Pages : 159

Get Book Here

Book Description
L'OBJECTIF DU TRAVAIL PRESENTE ICI EST D'AUGMENTER, PAR UN TRAITEMENT DE SURFACE, LA TENUE A L'OXYDATION A TEMPERATURE ELEVEE ET LA DURETE D'ACIERS FERRITIQUES FAIBLEMENT ALLIES. NOUS PRESENTONS LES RESULTATS OBTENUS AVEC LES ACIERS 35NCD16 ET Z38CDV5 PAR IRRADIATION LASER ASSURANT L'INCORPORATION SUPERFICIELLE ET LA DISSOLUTION DE PREDEPOTS DE NITRURES (ALN, SI#3N#4) OU DE CARBURES (SIC, CR#3C#2). NOUS PRECISIONS LES CONDITIONS D'OBTENTION D'ALLIAGES DE SURFACE EXEMPTS DE FISSURES, D'AMAS OU DE POROSITES. LA DURETE DE CES ALLIAGES DEPEND PRINCIPALEMENT DE LA FORMATION DE MARTENSITE ET (OU) DE LA PRECIPITATION DE CARBURES OU DE NITRURES. L'EXCELLENTE TENUE A L'OXYDATION EN CONDITIONS ISOTHERMES JUSQU'A 950C DE QUELQUES ALLIAGES DE SURFACE DANS UNE ATMOSPHERE D'OXYGENE RESULTE ESSENTIELLEMENT DE LA FORMATION D'UNE COUCHE D'OXYDE DE CHROME CR#2O#3. DANS LES ALLIAGES CONTENANT DU SILICIUM ET RELATIVEMENT PEU DE CHROME, LA CROISSANCE DE CETTE COUCHE DE CR#2O#3 N'INTERVIENT QU'APRES CELLE, INITIALE, D'UNE TRES MINCE PELLICULE DE SILICE QUI INHIBE L'OXYDATION DU FER ET REND POSSIBLE LE DEVELOPPEMENT DE LA COUCHE PROTECTRICE DE CR#2O#3. LE BON COMPORTEMENT EN CYCLAGE THERMIQUE DES ALLIAGES DE SURFACE ETUDIEES SUR L'ACIER Z38CDV5 RESULTERAIT DE LA CROISSANCE DE CR#2O#3 PAR DIFFUSION ANIONIQUE. LA PETITE TAILLE DE GRAINS DE CET OXYDE PERMETTRAIT UNE BONNE RELAXATION DE CONTRAINTES THERMIQUES PAR DEFORMATION PLASTIQUE. NOUS AVONS DONC MONTRE QUE LE TRAITEMENT LASER AVEC AJOUT PEUT CONSTITUER UN PROCEDE EFFICACE POUR CONFERER AUX ACIERS PEU ALLIES UN COMPORTEMENT EN OXYDATION A HAUTE TEMPERATURE TOUT A FAIT COMPARABLE A CELUI DES ACIERS INOXYDABLES AVEC L'AVANTAGE D'UNE DURETE PLUS ELEVEE

ETUDE DE L'OXYDATION A HAUTE TEMPERATURE DES REVETEMENTS NICRAIY ELABORES PAR TRAITEMENT LASER A PARTIR DE POUDRES PRE-ALLIEES - ANALYSE DES PARAMETRES STRUCTURAUX, PHYSICO-CHIMIQUES ET MECANIQUES

ETUDE DE L'OXYDATION A HAUTE TEMPERATURE DES REVETEMENTS NICRAIY ELABORES PAR TRAITEMENT LASER A PARTIR DE POUDRES PRE-ALLIEES - ANALYSE DES PARAMETRES STRUCTURAUX, PHYSICO-CHIMIQUES ET MECANIQUES PDF Author: FLAVIO SANDRO.. LAYS CASSINO
Publisher:
ISBN:
Category :
Languages : fr
Pages : 175

Get Book Here

Book Description
L'OBJET DE CE TRAVAIL EST D'ETUDIER LE COMPORTEMENT, SOUS OXYDATION ISOTHERME, D'ALLIAGES NICRAIY DANS LE DOMAINE DE TEMPERATURE ALLANT DE 800\C A 1200\C. CES ALLIAGES ONT ETE ELABORES, SOUS FORME DE REVETEMENTS DE SURFACE, PAR PROJECTION DE POUDRES PRE-ALLIEES AVEC FUSION PAR FAISCEAU LASER. DEUX REVETEMENTS, NI 6 4CR 2 5AL 1 0Y 0 . 2 ET NI 5 8CR 2 4AL 1 7Y 0 . 5, ONT ETE ANALYSES. L'ETUDE A PORTE SUR LES ASPECTS CINETIQUES, MORPHOLOGIQUES ET MECANIQUES DU PROCESSUS D'OXYDATION A HAUTE TEMPERATURE DES REVETEMENTS LASER ET, EN PARTICULIER, SUR LA RELATION ENTRE LA MICROSTRUCTURE TYPIQUE DE TELS ALLIAGES AVEC LA FORMATION ET LA TENUE MECANIQUE DE LA COUCHE D'OXYDE. LES RESULTATS OBTENUS POUR LES DEUX NUANCES MONTRENT QUE LE COMPORTEMENT GLOBAL, SOUS OXYDATION, EST ANALOGUE A CEUX, DEJA DECRIT DANS LA LITTERATURE, D'ALLIAGES DE COMPOSITIONS CHIMIQUES COMPARABLES A CELLES DES DEPOTS. LA COUCHE D'OXYDE EST FORMEE, ESSENTIELLEMENT, D'AL 2O 3, SOIT SOUS FORME STABLE (AL 2O 3), SOIT SOUS FORMES METASTABLES (AL 2O 3, AL 2O 3, ETC.). CEPENDANT, EN FONCTION DES CARACTERISTIQUES MICROSTRUCTURALES ET MICROCHIMIQUES DE CE TYPE DE REVETEMENT, DES DIFFERENCES IMPORTANTES ONT ETE MISES EN EVIDENCE. EN PARTICULIER, IL A ETE MONTRE QUE LE PROCESSUS DE DEPOT INDUIT UNE DISTRIBUTION EN YTTRIUM CAPABLE D'AFFECTER LE DEVELOPPEMENT DE LA COUCHE D'ALUMINE DES LE DEBUT DU PROCESSUS D'OXYDATION. DES REGIONS DE DECOLLEMENT D'OXYDE ONT ETE MISES EN RELATION AVEC LA DISTRIBUTION EN YTTRIUM. EN DESSUS DE 1000\C CES DECOLLEMENTS D'OXYDE N'ONT PAS ETE OBSERVES ; TEMOIGNANT UN MECANISME DE CICATRISATION. L'EXISTENCE D'UNE VAPORISATION A HAUTE TEMPERATURE A ETE IDENTIFIEE, QUI PEUT JOUER SUR LA RELAXATION DES CONTRAINTES. LES CONTRAINTES RESIDUELLES APRES

ALLIAGES DE SURFACE RENFORCES PAR DES CARBURES ELABORES PAR IRRADIATION LASER SUR L'ACIER INOXYDABLE AISI 316L

ALLIAGES DE SURFACE RENFORCES PAR DES CARBURES ELABORES PAR IRRADIATION LASER SUR L'ACIER INOXYDABLE AISI 316L PDF Author: FRANCK.. LAROUDIE
Publisher:
ISBN:
Category :
Languages : fr
Pages : 210

Get Book Here

Book Description
DES ALLIAGES DE SURFACE RENFORCES PAR DES CARBURES MIXTES FER-CHROME M#7C#3 (M = FE, CR) D'UNE PART, ET PAR DU CARBURE DE TITANE D'AUTRE PART, ONT ETE ELABORES PAR IRRADIATION LASER SUR L'ACIER INOXYDABLE AUSTENITIQUE AISI 316L (Z2 CND 17-12) AFIN D'AMELIORER SA RESISTANCE A L'USURE. L'UTILISATION DE DIFFERENTS PRECURSEURS (GRAPHITE, CARBURE DE SILICIUM, CARBURE CR#3C#2 SEUL OU ASSOCIE A DU CHROME, TIC SUBMICRONIQUE ET MICRONIQUE, MELANGE DE POUDRES DE TITANE ET DE CARBURE SIC) A PERMIS D'OBTENIR DES REVETEMENTS PRESENTANT UNE LARGE VARIETE DE MICROSTRUCTURES ET DE COMPOSITIONS. LES MICRODURETES CORRESPONDANTES, COMPRISES ENTRE 350 HV ET 900 HV TEMOIGNENT D'UN DURCISSEMENT SIGNIFICATIF DE L'ACIER 316L (200 HV). LA CONFRONTATION DES PHASES PRESENTES DANS LES DIFFERENTS ALLIAGES DE SURFACE AVEC CELLES DES DIAGRAMMES D'EQUILIBRE DES SYSTEMES CORRESPONDANTS A MIS EN EVIDENCE LE CARACTERE METASTABLE DES CARBURES M#7C#3 ET LA BONNE STABILITE THERMIQUE DES CARBURES DE TITANE. LA RESISTANCE A L'OXYDATION A HAUTE TEMPERATURE DES DIVERS ALLIAGES DE SURFACE A ETE CARACTERISEE PAR THERMOGRAVIMETRIE. LES RESULTATS OBTENUS ONT MONTRE LE ROLE ESSENTIEL DES ELEMENTS CHROME ET SILICIUM DANS LE PROCESSUS D'OXYDATION. AINSI, LES REVETEMENTS ELABORES PAR IRRADIATION D'UN MELANGE DE CARBURE CR#3C#2 ET DE CHROME, ET CEUX OBTENUS A PARTIR D'UN PREDEPOT CONSTITUE D'UN MELANGE DE TITANE ET DE CARBURE DE SILICIUM, PRESENTENT UNE EXCELLENTE RESISTANCE A L'OXYDATION A 1000C, EQUIVALENTE A CELLE DE L'ACIER 316L. D'AUTRE PART, LE MAINTIEN PROLONGE A 1000C DES ALLIAGES CONTENANT DES CARBURES M#7C#3 CONDUIT A LA PRECIPITATION DES PHASES D'EQUILIBRE CE QUI PROVOQUE UNE NETTE BAISSE DE DURETE. AUCUNE MODIFICATION STRUCTURALE N'EST OBSERVEE DANS LES ALLIAGES CONTENANT DES CARBURES DE TITANE. LES TESTS DE CORROSION INTERGRANULAIRE EFFECTUES ONT CONFIRME LE ROLE PREPONDERANT DU CHROME SUR LE COMPORTEMENT A LA CORROSION. ENFIN, LES TESTS D'USURE PAR FROTTEMENT EFFECTUES SUR CES DIFFERENTS ALLIAGES DE SURFACE ONT MONTRE QUE LE DURCISSEMENT OBTENU PERMET UNE AMELIORATION SIGNIFICATIVE DU COMPORTEMENT TRIBOLOGIQUE DE L'ACIER 316L