Thermal Effects on the Mechanical Properties of SiC Fiber Reinforced Reaction Bonded Silicon Nitride Matrix (SiC/RBSN) Composites

Thermal Effects on the Mechanical Properties of SiC Fiber Reinforced Reaction Bonded Silicon Nitride Matrix (SiC/RBSN) Composites PDF Author: R. T. Bhatt
Publisher:
ISBN:
Category :
Languages : en
Pages : 20

Get Book Here

Book Description
The elevated temperature four-point flexural strength and the room temperature tensile and flexural strength properties after thermal shock were measured for ceramic composites consisting of 30 vol % uniaxially aligned 142 microns diameter SiC fibers in a reaction bonded Si3N4 matrix. The elevated temperature strengths were measured after 15 min of exposure in air at temperatures to 1400 C. The thermal shock treatment was accomplished by heating the composite in air for 15 min at temperatures to 1200 C and then quenching in water at 25 C. The results indicate no significant loss in strength properties either at temperature or after thermal shock when compared with the strength data for composites in the as-fabricated condition. (jes).