Qualitative TEM analysis revealed that PWA 1484 deformed by large dislocation "ribbons" spanning large regions of material. PWA 1480, however, deformed primarily due to matrix dislocations and the creation of interfacial dislocation networks between the [gamma] and [gamma]' phases. PWA 1480+ contained stacking faults as well, though they acted on multiple slip systems generating work hardening and forcing the onset of secondary creep. Xray diffraction and JMatPro calculations were also used to gain insight into the cause of the differences in behaviors.
The Primary Creep Behavior of Single Crystal, Nickel Base Superalloys PWA 1480 and PWA 1484
Author: Brandon Charles Wilson
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
Qualitative TEM analysis revealed that PWA 1484 deformed by large dislocation "ribbons" spanning large regions of material. PWA 1480, however, deformed primarily due to matrix dislocations and the creation of interfacial dislocation networks between the [gamma] and [gamma]' phases. PWA 1480+ contained stacking faults as well, though they acted on multiple slip systems generating work hardening and forcing the onset of secondary creep. Xray diffraction and JMatPro calculations were also used to gain insight into the cause of the differences in behaviors.
Publisher:
ISBN:
Category :
Languages : en
Pages :
Book Description
Qualitative TEM analysis revealed that PWA 1484 deformed by large dislocation "ribbons" spanning large regions of material. PWA 1480, however, deformed primarily due to matrix dislocations and the creation of interfacial dislocation networks between the [gamma] and [gamma]' phases. PWA 1480+ contained stacking faults as well, though they acted on multiple slip systems generating work hardening and forcing the onset of secondary creep. Xray diffraction and JMatPro calculations were also used to gain insight into the cause of the differences in behaviors.
Elevated Temperature Tension, Compression and Creep-rupture Behavior of (001)-oriented Single Crystal Superalloy PWA 1480
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages : 26
Book Description
Publisher:
ISBN:
Category :
Languages : en
Pages : 26
Book Description
Yielding and Deformation Behavior of the Single Crystal Nickel-Base Superalloy PWA 1480
Author:
Publisher:
ISBN:
Category :
Languages : en
Pages : 96
Book Description
Interrupted tensile tests were conducted to fixed plastic strain levels in 001 oriented single crystals of the nickel-base superalloys PWA 1480. Testing was done in the range from 20-1093 C, at strain rates of 0.5 and 50%/min. The yield strength was constant from 20-760 C, above which the strength dropped rapidly and became a strong function of strain rate. The high temperature data could be represented very well by an Arrhenius-type equation, which resulted in three distinct temperature regimes. The deformation substructures could be grouped in the same three regimes.
Publisher:
ISBN:
Category :
Languages : en
Pages : 96
Book Description
Interrupted tensile tests were conducted to fixed plastic strain levels in 001 oriented single crystals of the nickel-base superalloys PWA 1480. Testing was done in the range from 20-1093 C, at strain rates of 0.5 and 50%/min. The yield strength was constant from 20-760 C, above which the strength dropped rapidly and became a strong function of strain rate. The high temperature data could be represented very well by an Arrhenius-type equation, which resulted in three distinct temperature regimes. The deformation substructures could be grouped in the same three regimes.
Yielding and Deformation Behavior of the Single Crystal Nickel-Base Superalloy PWA 1480
Author: Walter W Mulligan (Jr)
Publisher:
ISBN:
Category : Dislocations in crystals
Languages : en
Pages : 90
Book Description
Interrupted tensile tests were conducted to fixed plastic strain levels in 001 oriented single crystals of the nickel-base superalloys PWA 1480. Testing was done in the range from 20-1093 C, at strain rates of 0.5 and 50%/min. The yield strength was constant from 20-760 C, above which the strength dropped rapidly and became a strong function of strain rate. The high temperature data could be represented very well by an Arrhenius-type equation, which resulted in three distinct temperature regimes. The deformation substructures could be grouped in the same three regimes.
Publisher:
ISBN:
Category : Dislocations in crystals
Languages : en
Pages : 90
Book Description
Interrupted tensile tests were conducted to fixed plastic strain levels in 001 oriented single crystals of the nickel-base superalloys PWA 1480. Testing was done in the range from 20-1093 C, at strain rates of 0.5 and 50%/min. The yield strength was constant from 20-760 C, above which the strength dropped rapidly and became a strong function of strain rate. The high temperature data could be represented very well by an Arrhenius-type equation, which resulted in three distinct temperature regimes. The deformation substructures could be grouped in the same three regimes.
Mechanical Properties and Performance of Engineering Ceramics and Composites XI, Volume 37, Issue 2
Author: Jonathan Salem
Publisher: John Wiley & Sons
ISBN: 1119320143
Category : Technology & Engineering
Languages : en
Pages : 331
Book Description
A collection of 23 papers from The American Ceramic Society's 40th International Conference on Advanced Ceramics and Composites, held in Daytona Beach, Florida, January 24-29, 2016. This issue includes papers presented in Symposium 1 - Mechanical Behavior and Performance of Ceramics and Composites.
Publisher: John Wiley & Sons
ISBN: 1119320143
Category : Technology & Engineering
Languages : en
Pages : 331
Book Description
A collection of 23 papers from The American Ceramic Society's 40th International Conference on Advanced Ceramics and Composites, held in Daytona Beach, Florida, January 24-29, 2016. This issue includes papers presented in Symposium 1 - Mechanical Behavior and Performance of Ceramics and Composites.
Superalloys 2024
Author: Jonathan Cormier
Publisher: Springer Nature
ISBN: 3031639375
Category :
Languages : en
Pages : 1121
Book Description
Publisher: Springer Nature
ISBN: 3031639375
Category :
Languages : en
Pages : 1121
Book Description
Creep and Microstructural Stability of Ruthenium-containing Nickel-base Single Crystal Superalloys
Author: Laura Jill Rowland
Publisher:
ISBN:
Category :
Languages : en
Pages : 486
Book Description
Publisher:
ISBN:
Category :
Languages : en
Pages : 486
Book Description
Yielding and Deformation Behavior of the Single Crystal Superalloy PWA 1480
Author: Walter W. Milligan
Publisher:
ISBN:
Category : Strengthening mechanisms in solids
Languages : en
Pages : 182
Book Description
Publisher:
ISBN:
Category : Strengthening mechanisms in solids
Languages : en
Pages : 182
Book Description
An Analysis of Primary Creep of Nickel-base Superalloy Single Crystals
Author: P. R. PASLAY
Publisher:
ISBN:
Category :
Languages : en
Pages : 6
Book Description
Publisher:
ISBN:
Category :
Languages : en
Pages : 6
Book Description
Dissertation Abstracts International
Author:
Publisher:
ISBN:
Category : Dissertations, Academic
Languages : en
Pages : 800
Book Description
Publisher:
ISBN:
Category : Dissertations, Academic
Languages : en
Pages : 800
Book Description