Iodine stress corrosion cracking of as-received Zircaloy-4 at 700 [degrees] C and 800 [degrees] C

Iodine stress corrosion cracking of as-received Zircaloy-4 at 700 [degrees] C and 800 [degrees] C PDF Author: D. Lim
Publisher:
ISBN:
Category :
Languages : en
Pages : 0

Get Book Here

Book Description

Iodine stress corrosion cracking of as-received Zircaloy-4 at 700 [degrees] C and 800 [degrees] C

Iodine stress corrosion cracking of as-received Zircaloy-4 at 700 [degrees] C and 800 [degrees] C PDF Author: D. Lim
Publisher:
ISBN:
Category :
Languages : en
Pages : 0

Get Book Here

Book Description


Iodine stress corrosion cracking of as-received zircaloy-4 at 700 degrees centigrade and 800 degrees centigrade

Iodine stress corrosion cracking of as-received zircaloy-4 at 700 degrees centigrade and 800 degrees centigrade PDF Author: D. Lim
Publisher:
ISBN:
Category :
Languages : en
Pages : 0

Get Book Here

Book Description
The effects of iodine stress corrosion cracking (iscc) on the rupture behaviour of candu fuel sheathings at temperatures of 700 degrees c and 800 degrees c in isothermal hold tests were investigated under inert gas conditions. the sheaths were tested in the as-received condition with no braze zones or appendages . a test apparatus and specimen design were developed to provide an environment suitable for iscc during high temperature transient conditions. the burst tests showed that the deformation behaviour of the zircaloy tubes was not influenced by the presence of iodine at 800 degrees c at hoop stresses between 15 mpa-35 mpa, when subjected to temperature ramps of approximately 30 degrees c/s. iscc were observed at 700 degrees c at hoop stresses of 40-60-mpa. a three-fold reduction in sheath strain was observed in specimens which failed by iscc when compared with reference specimens containing no iodine. no significant difference in time-to-failure was observed between the reference specimens and the iodine specimens at both temperatures.

Iodine stress corrosion cracking of as-received zircaloy-4 at 700 degrees celsius and 800 degrees celsius

Iodine stress corrosion cracking of as-received zircaloy-4 at 700 degrees celsius and 800 degrees celsius PDF Author: D. Lim
Publisher:
ISBN:
Category :
Languages : en
Pages : 0

Get Book Here

Book Description


Laboratory study of stress corrosion cracking of zircaloy-2 in iodine at 300 degrees c

Laboratory study of stress corrosion cracking of zircaloy-2 in iodine at 300 degrees c PDF Author: J. C. Wood
Publisher:
ISBN:
Category :
Languages : en
Pages : 0

Get Book Here

Book Description


Influence of Iodine on the Strain and Rupture Behavior of Zircaloy-4 Cladding Tubes at High Temperatures

Influence of Iodine on the Strain and Rupture Behavior of Zircaloy-4 Cladding Tubes at High Temperatures PDF Author: P. Hofmann
Publisher:
ISBN:
Category : Burst tests
Languages : en
Pages : 20

Get Book Here

Book Description
The stress corrosion cracking (SCC) behavior of short tubular Zircaloy-4 specimens by the action of iodine (initial iodine concentration: 0.1 to 10 mg/cm3) was investigated out-of-pile between 600 and 1100°C under inert gas conditions. The Zircaloy cladding tube was used as-received and with an inner preliminary oxidation. Moreover, the influence of the uranium oxide (UO2) oxygen potential on the SCC behavior was studied.

The effects of three different coatings on iodine-induced stress-corrosion cracking of zircaloy-4

The effects of three different coatings on iodine-induced stress-corrosion cracking of zircaloy-4 PDF Author: B. A. Surette
Publisher:
ISBN:
Category :
Languages : en
Pages : 0

Get Book Here

Book Description


Iodine Stress-corrosion Cracking in Irradiated Zircaloy Cladding. [PWR ; BWR].

Iodine Stress-corrosion Cracking in Irradiated Zircaloy Cladding. [PWR ; BWR]. PDF Author:
Publisher:
ISBN:
Category :
Languages : en
Pages :

Get Book Here

Book Description
Irradiated Zircaloy cladding specimens, which had experienced fluences from 0.1 to 6 x 1021 n/cm2 (E>0.1 MeV), were gas-pressure tested in an iodine environment to investigate their stress-corrosion cracking (SCC) susceptibility. The test temperatures and hoop stresses ranged from 320 to 360°C and 150 to 500 MPa, respectively. The results indicate that irradiation, in general, increases the susceptibility of Zircaloy to iodine SCC. For specimens that experienced fluences>2 x 1021 n/cm2 (E>0.1 MeV), the 24-h failure stress was 177+-18 MPa, regardless of the preirradiation metallurgical condition. An analytical model for iodine SCC has been developed which agrees reasonably well with the test results.

Energy Research Abstracts

Energy Research Abstracts PDF Author:
Publisher:
ISBN:
Category : Power resources
Languages : en
Pages : 500

Get Book Here

Book Description


Grain-by-Grain Study of the Mechanisms of Crack Propagation During Iodine Stress Corrosion Cracking of Zircaloy-4

Grain-by-Grain Study of the Mechanisms of Crack Propagation During Iodine Stress Corrosion Cracking of Zircaloy-4 PDF Author: AO. Dorado
Publisher:
ISBN:
Category : Applied stress
Languages : en
Pages : 17

Get Book Here

Book Description
This paper describes the tests conducted to determine the conditions leading to cracking of a specified grain of metal, during the iodine stress corrosion cracking (SCC) of zirconium alloys, focusing on the crystallographic orientation of crack paths, the critical stress conditions, and the significance of the fractographic features encountered. In order to perform crystalline orientation of fracture surfaces, a specially heat-treated Zircaloy-4 having very large grains, grown up to the wall thickness, was used. Careful orientation work has proved that intracrystalline pseudo-cleavage occurs only along basal planes. The effects of anisotropy, plasticity, triaxiality, and residual stresses originated in thermal contraction have to be considered to account for the influence of the stress state. A grain-by-grain calculation led to the conclusion that transgranular cracking always takes place on those bearing the maximum resolved tensile stress perpendicular to basal planes. Propagation along twin boundaries has been identified among the different fracture modes encountered.

Iodine-Induced Stress Corrosion of Zircaloy Fuel Cladding

Iodine-Induced Stress Corrosion of Zircaloy Fuel Cladding PDF Author: L. Brunisholz
Publisher:
ISBN:
Category : Crack propagation
Languages : en
Pages : 17

Get Book Here

Book Description
Because of its impact on nuclear power plant reliability, fuel cladding failure induced by pellet cladding interaction is a problem of major concern. It is usually analyzed as stress corrosion cracking caused by volatile fission products like iodine.