A Summary of Comparative Properties of Air-melted and Vacuum-melted Steels and Superalloys

A Summary of Comparative Properties of Air-melted and Vacuum-melted Steels and Superalloys PDF Author: D. C. Ludwigson
Publisher:
ISBN:
Category : Heat resistant alloys
Languages : en
Pages : 158

Get Book Here

Book Description


Superalloy Forgings

Superalloy Forgings PDF Author: H. J. Henning
Publisher:
ISBN:
Category : Heat resistant alloys
Languages : en
Pages : 48

Get Book Here

Book Description


Nuclear Science Abstracts

Nuclear Science Abstracts PDF Author:
Publisher:
ISBN:
Category : Nuclear energy
Languages : en
Pages : 1220

Get Book Here

Book Description


Catalog of Technical Reports

Catalog of Technical Reports PDF Author: United States. Dept. of Commerce. Office of Technical Services
Publisher:
ISBN:
Category :
Languages : en
Pages : 850

Get Book Here

Book Description


High-strength-steel Forgings

High-strength-steel Forgings PDF Author: H. J. Henning
Publisher:
ISBN:
Category : Blacksmithing
Languages : en
Pages : 68

Get Book Here

Book Description
THIS REPORT IS MAINLY CONCERNED WITH FORGINGS MADE FROM MARTENSITIC STEELS HEAT TREATED TO STRENGTHS RANGING FROM 240,000 TO 300,000 PSI. FORGING CHARACTERISTICS, DESIGN LIMITATIONS, DIMENSIONAL TOLERANCES, AND QUALITY-CONTROL PROBLEMS ARE DISCUSSED. A CONSIDERABLE AMOUNT OF DATA ON MECHANICAL PROPERTIES IS ALSO PRESENTED. IN ADDITION, THE REPORT SUMMARIZES THE AVAILABLE INFORMATION ON FORGED, SEMIAUSTENITIAL STEELS. THIS COMPILATION IS BASED ON PUBLISHED ARTICLES, GOVERNMENT REPORTS, AND INTERVIEWS WITH PRODUCERS AND USERS OF STEEL FORGINGS.

Melting and Casting of the Refractory Metals Molybdenum, Columbium, Tantalum, and Tungsten

Melting and Casting of the Refractory Metals Molybdenum, Columbium, Tantalum, and Tungsten PDF Author: W. H. Johnson
Publisher:
ISBN:
Category : Heat resistant alloys
Languages : en
Pages : 42

Get Book Here

Book Description


U.S. Government Research Reports

U.S. Government Research Reports PDF Author:
Publisher:
ISBN:
Category : Science
Languages : en
Pages : 950

Get Book Here

Book Description


Vacuum Degassing in the Production of Premium-quality Steels

Vacuum Degassing in the Production of Premium-quality Steels PDF Author: P. J. O'Reilly
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 138

Get Book Here

Book Description
This report gives the experiences of several steel producers and consumers with vacuum degassing as a melting practice in the manufacture of high-strength steels for critical applications. The parameters involved in determining the effects of melting practice on mechanical properties are outlined. Pertinent melting processes are described and evaluated qualitatively. In presenting the data, vacuum degassing is compared with other melting practices such as conventional air melting and consumable-electrode vacuum-arc remelting (CEVAR). Generally, there is a trend indicating that vacuum degassing is being used in some production applications instead of air-melted or CEVAR material. In terms of higher and more uniform transverse tensile properties and impact strength, longer fatigue life, and improved cleanliness, the CEVAR alloys were the best. Vacuum degassing by any of the various methods resulted in an improvement in properties of air-melted alloys. In some instances it appeared that the quality of CEVAR alloys could be approached when stream degassing or D-H (Dortmund-Horder) treatment was applied to air melts. Recommendations are given for additional investigations on the effects of melting practice on mechanical properties of premium-quality steels. (Author).

An Overall Study of Partial Denture Alloys

An Overall Study of Partial Denture Alloys PDF Author: Kamal Asgar
Publisher:
ISBN:
Category : Dental metallurgy
Languages : en
Pages : 388

Get Book Here

Book Description


Physical and Mechanical Properties of Commercial Molybdenum-base Alloys

Physical and Mechanical Properties of Commercial Molybdenum-base Alloys PDF Author: J. A. Houck
Publisher:
ISBN:
Category : Molybdenum
Languages : en
Pages : 196

Get Book Here

Book Description