Author: NAVAL APPLIED SCIENCE LAB BROOKLYN N Y.
Publisher:
ISBN:
Category :
Languages : en
Pages : 10
Book Description
The results of this investigation indicates that mechanized out-of-chamber welding of thick plate titanium alloy in the flat position can be accomplished without undue difficulty, provided that care is exercised in the preparation of the plates for welding and in the control of the welding operation and that a trailing shield of suitable design is used in the operation. Additional work in out-of-chamber mechanized welding of thick plate titanium is required to establish appropriate welding conditions for specific alloys intended for use in submarine hull construction and to assess the properties of weldments produced with these alloys.
Development of Welding Procedures for the Fabrication of Thick Plate Titanium Alloy
Author: NAVAL APPLIED SCIENCE LAB BROOKLYN N Y.
Publisher:
ISBN:
Category :
Languages : en
Pages : 10
Book Description
The results of this investigation indicates that mechanized out-of-chamber welding of thick plate titanium alloy in the flat position can be accomplished without undue difficulty, provided that care is exercised in the preparation of the plates for welding and in the control of the welding operation and that a trailing shield of suitable design is used in the operation. Additional work in out-of-chamber mechanized welding of thick plate titanium is required to establish appropriate welding conditions for specific alloys intended for use in submarine hull construction and to assess the properties of weldments produced with these alloys.
Publisher:
ISBN:
Category :
Languages : en
Pages : 10
Book Description
The results of this investigation indicates that mechanized out-of-chamber welding of thick plate titanium alloy in the flat position can be accomplished without undue difficulty, provided that care is exercised in the preparation of the plates for welding and in the control of the welding operation and that a trailing shield of suitable design is used in the operation. Additional work in out-of-chamber mechanized welding of thick plate titanium is required to establish appropriate welding conditions for specific alloys intended for use in submarine hull construction and to assess the properties of weldments produced with these alloys.
Development of Welding Techniques for Fabricating a Thick Plate Titanium Pressure Box
Author: NAVAL APPLIED SCIENCE LAB BROOKLYN N Y.
Publisher:
ISBN:
Category :
Languages : en
Pages : 17
Book Description
Suitable out-of-chamber, manual and semi-automatic welding techniques have been developed for the fabrication of a titanium alloy pressure box of the type required for low cycle fatigue studies at the Marine Engineering Laboratory. These techniques may also be used for fabricating complex structural elements of heavy plate titanium. (Author).
Publisher:
ISBN:
Category :
Languages : en
Pages : 17
Book Description
Suitable out-of-chamber, manual and semi-automatic welding techniques have been developed for the fabrication of a titanium alloy pressure box of the type required for low cycle fatigue studies at the Marine Engineering Laboratory. These techniques may also be used for fabricating complex structural elements of heavy plate titanium. (Author).
Recent Developments in Welding Thick Titanium Plate
Author: R. E. Monroe
Publisher:
ISBN:
Category : Titanium
Languages : en
Pages : 26
Book Description
This memorandum represents a combined effort by the U.S. Naval Applied Science Laboratory, Brooklyn, New York, and the Defense Metals Information Center to summarize new information on welding thick Ti plate. Thick plate of Ti continues to be of interest to the aerospace and defense industries for possible use in submersibles, armored vehicles, large space boosters, high-speed aircraft, and for pressure vessels. This memorandum generally is limited to information on welding Ti plate that is (1) at least 1 in. thick and (2) that is not covered by DMIC Report 185, The Status and Properties of Titanium Alloys for Thick Plate, June 14, 1963. The general requirements for welding Ti are not repeated here, since they are well documented in references mentioned in the inroduction to the memorandum. Sections have been prepared to cover material developments, welding-process developments, weld properties, and residual welding stresses. (Author).
Publisher:
ISBN:
Category : Titanium
Languages : en
Pages : 26
Book Description
This memorandum represents a combined effort by the U.S. Naval Applied Science Laboratory, Brooklyn, New York, and the Defense Metals Information Center to summarize new information on welding thick Ti plate. Thick plate of Ti continues to be of interest to the aerospace and defense industries for possible use in submersibles, armored vehicles, large space boosters, high-speed aircraft, and for pressure vessels. This memorandum generally is limited to information on welding Ti plate that is (1) at least 1 in. thick and (2) that is not covered by DMIC Report 185, The Status and Properties of Titanium Alloys for Thick Plate, June 14, 1963. The general requirements for welding Ti are not repeated here, since they are well documented in references mentioned in the inroduction to the memorandum. Sections have been prepared to cover material developments, welding-process developments, weld properties, and residual welding stresses. (Author).
U. S. Government Research and Development Reports
Author:
Publisher:
ISBN:
Category : Science
Languages : en
Pages : 1776
Book Description
Publisher:
ISBN:
Category : Science
Languages : en
Pages : 1776
Book Description
Technical Abstract Bulletin
Author:
Publisher:
ISBN:
Category : Science
Languages : en
Pages : 908
Book Description
Publisher:
ISBN:
Category : Science
Languages : en
Pages : 908
Book Description
Research and Development for the Welding of Titanium and Titanium Alloys
Author: J. J. Chyle
Publisher:
ISBN:
Category : Titanium
Languages : en
Pages : 94
Book Description
Publisher:
ISBN:
Category : Titanium
Languages : en
Pages : 94
Book Description
Advances in Welding Technologies for Process Development
Author: Jaykumar Vora
Publisher: CRC Press
ISBN: 1351234803
Category : Technology & Engineering
Languages : en
Pages : 317
Book Description
Within manufacturing, welding is by far the most widely used fabrication method used for production, leading to a rise in research and development activities pertaining to the welding and joining of different, similar, and dissimilar combinations of the metals. This book addresses recent advances in various welding processes across the domain, including arc welding and solid-state welding process, as well as experimental processes. The content is structured to update readers about the working principle, predicaments in existing process, innovations to overcome these problems, and direct industrial and practical applications. Key Features: Describes recent developments in welding technology, engineering, and science Discusses advanced computational techniques for procedure development Reviews recent trends of implementing DOE and meta-heuristics optimization techniques for setting accurate parameters Addresses related theoretical, practical, and industrial aspects Includes all the aspects of welding, such as arc welding, solid state welding, and weld overlay
Publisher: CRC Press
ISBN: 1351234803
Category : Technology & Engineering
Languages : en
Pages : 317
Book Description
Within manufacturing, welding is by far the most widely used fabrication method used for production, leading to a rise in research and development activities pertaining to the welding and joining of different, similar, and dissimilar combinations of the metals. This book addresses recent advances in various welding processes across the domain, including arc welding and solid-state welding process, as well as experimental processes. The content is structured to update readers about the working principle, predicaments in existing process, innovations to overcome these problems, and direct industrial and practical applications. Key Features: Describes recent developments in welding technology, engineering, and science Discusses advanced computational techniques for procedure development Reviews recent trends of implementing DOE and meta-heuristics optimization techniques for setting accurate parameters Addresses related theoretical, practical, and industrial aspects Includes all the aspects of welding, such as arc welding, solid state welding, and weld overlay
Government-wide Index to Federal Research & Development Reports
Author:
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages : 1288
Book Description
Publisher:
ISBN:
Category : Government publications
Languages : en
Pages : 1288
Book Description
Development of Procedures for Welding 2-inch-thick Titanium-alloy Plate
Author: R. L. KOPPENHOFER
Publisher:
ISBN:
Category :
Languages : en
Pages : 21
Book Description
Procedures for welding 2-inch-thick Ti-alloy plate were developed for 4 alloys: commercially pure titanium, Ti-6Al-4V, Ti-5Al-2.5Sn, and Ti-13V-11Cr-3Al. Commercially available filler wires and experimental filler materials were used make the welds. The properties of the welds were generally as good as or better than those of the base plate. The results show that heavy titanium-alloy plates can be satisfactorily welded provided they are adequately protected from weld contamination and the compositions of the filler wire and base plate are properly controlled. A controlled-atmosphere welding chamber was used to provide protection for the welds in this program. The impact properties of the base plate did not meet the requirements for submarine hulls, but two of the alloys show promise: Ti-6Al-4V and the Ti-5Al-2.5Sn alloys. (Author).
Publisher:
ISBN:
Category :
Languages : en
Pages : 21
Book Description
Procedures for welding 2-inch-thick Ti-alloy plate were developed for 4 alloys: commercially pure titanium, Ti-6Al-4V, Ti-5Al-2.5Sn, and Ti-13V-11Cr-3Al. Commercially available filler wires and experimental filler materials were used make the welds. The properties of the welds were generally as good as or better than those of the base plate. The results show that heavy titanium-alloy plates can be satisfactorily welded provided they are adequately protected from weld contamination and the compositions of the filler wire and base plate are properly controlled. A controlled-atmosphere welding chamber was used to provide protection for the welds in this program. The impact properties of the base plate did not meet the requirements for submarine hulls, but two of the alloys show promise: Ti-6Al-4V and the Ti-5Al-2.5Sn alloys. (Author).
Bibliography of Scientific and Industrial Reports
Author:
Publisher:
ISBN:
Category : Technology
Languages : en
Pages : 1698
Book Description
Publisher:
ISBN:
Category : Technology
Languages : en
Pages : 1698
Book Description