Threshold Crack Growth Behavior of Nickel-Base Superalloy at Elevated Temperature

Threshold Crack Growth Behavior of Nickel-Base Superalloy at Elevated Temperature PDF Author: NE. Ashbaugh
Publisher:
ISBN:
Category : Crack arrest
Languages : en
Pages : 11

Get Book Here

Book Description
An experimental program was conducted to evaluate the effects of frequency and R on the near-threshold crack growth behavior of Inconel 718 at 649°C in laboratory air. Frequencies from 0.01 to 400 Hz and R from 0.1 to 0.9 were applied to compact tension [C(T)] and middle- or center-cracked tension [M(T)] specimens under decreasing-K conditions using computer-controlled test machines. Digital load-displacement data were obtained to determine crack length and closure load. The fatigue crack growth threshold in Inconel 718 at 649°C obtained using decreasing ?K testing was generally associated with a crack arrest phenomenon which could be attributed to the buildup of oxides with time. Over the ranges of R and v used in this investigation, the growth rate behavior at the onset of crack arrest appears to be a combination of time-dependent and cyclic-dependent behavior. Even at 400 Hz, purely cyclic behavior was apparently never reached. For crack growth rate modeling, both frequency and stress ratio have to be incorporated in the characterization of ?Kth. Over the ranges of parameters tested, a cyclic threshold was approached at high frequencies and low R and a sustained load time-dependent threshold was obtained at high R, indicating that the cyclic contribution to the growth rate was negligible.

Threshold Crack Growth Behavior of Nickel-Base Superalloy at Elevated Temperature

Threshold Crack Growth Behavior of Nickel-Base Superalloy at Elevated Temperature PDF Author: NE. Ashbaugh
Publisher:
ISBN:
Category : Crack arrest
Languages : en
Pages : 11

Get Book Here

Book Description
An experimental program was conducted to evaluate the effects of frequency and R on the near-threshold crack growth behavior of Inconel 718 at 649°C in laboratory air. Frequencies from 0.01 to 400 Hz and R from 0.1 to 0.9 were applied to compact tension [C(T)] and middle- or center-cracked tension [M(T)] specimens under decreasing-K conditions using computer-controlled test machines. Digital load-displacement data were obtained to determine crack length and closure load. The fatigue crack growth threshold in Inconel 718 at 649°C obtained using decreasing ?K testing was generally associated with a crack arrest phenomenon which could be attributed to the buildup of oxides with time. Over the ranges of R and v used in this investigation, the growth rate behavior at the onset of crack arrest appears to be a combination of time-dependent and cyclic-dependent behavior. Even at 400 Hz, purely cyclic behavior was apparently never reached. For crack growth rate modeling, both frequency and stress ratio have to be incorporated in the characterization of ?Kth. Over the ranges of parameters tested, a cyclic threshold was approached at high frequencies and low R and a sustained load time-dependent threshold was obtained at high R, indicating that the cyclic contribution to the growth rate was negligible.

Near-Threshold Crack Growth in Nickel-Base Superalloys

Near-Threshold Crack Growth in Nickel-Base Superalloys PDF Author: HR. Van Stone
Publisher:
ISBN:
Category : Crack closure
Languages : en
Pages : 24

Get Book Here

Book Description
The influence of stress ratio on the elevated-temperature crack growth behavior of the nickel-base superalloys René 95 and Alloy 718 is discussed. The near-threshold and Region II crack growth behavior of a wide variety of microstructures for each alloy are explained using phenomenological descriptions of closure, that is, K-dependent or K-independent closure. K-dependent closure is the type of closure observed for nickel-base superalloys where increasing the R-ratio causes a uniform lateral shift of the entire fatigue crack growth curve. K-independent closure is the type commonly reported for steels and titanium alloys where increasing the R-ratio has a larger influence on near-threshold crack growth than on Region II crack growth. The existence of K-dependent closure in nickel-base superalloys results in microstructurally sensitive crack growth rates, even at high R-ratios. This permits the use of K-based crack growth prediction techniques and simplifies alloy and process development for applications having complex loading spectra.

The Near Threshold Fatigue Crack Growth Behavior of a Nickel-based Superalloy

The Near Threshold Fatigue Crack Growth Behavior of a Nickel-based Superalloy PDF Author: George John Gikas
Publisher:
ISBN:
Category : Alloys
Languages : en
Pages : 0

Get Book Here

Book Description


Superalloys 2012

Superalloys 2012 PDF Author: Eric S. Huron
Publisher: John Wiley & Sons
ISBN: 1118516400
Category : Technology & Engineering
Languages : en
Pages : 952

Get Book Here

Book Description
A superalloy, or high-performance alloy, is an alloy that exhibits excellent mechanical strength at high temperatures. Superalloy development has been driven primarily by the aerospace and power industries. This compilation of papers from the Twelfth International Symposium on Superalloys, held from September 9-13, 2012, offers the most recent technical information on this class of materials.

The Effects of Carburizing Environments on Elevated Temperature Fatigue Crack Growth Behavior in the Nickel-base Superalloy Nimonic 115

The Effects of Carburizing Environments on Elevated Temperature Fatigue Crack Growth Behavior in the Nickel-base Superalloy Nimonic 115 PDF Author: Carl J. White
Publisher:
ISBN:
Category : Heat resistant alloys
Languages : en
Pages : 222

Get Book Here

Book Description


Elevated Temperature Fatigue Crack Growth in a Nickel Base Superalloy Under Dwell Conditions

Elevated Temperature Fatigue Crack Growth in a Nickel Base Superalloy Under Dwell Conditions PDF Author: J. Byrne
Publisher:
ISBN:
Category : Materials
Languages : en
Pages :

Get Book Here

Book Description


Near Threshold Corrosion Fatigue Crack Growth Behavior of a Nickel Base Superalloy in Air and Inert Environments

Near Threshold Corrosion Fatigue Crack Growth Behavior of a Nickel Base Superalloy in Air and Inert Environments PDF Author: James Lum Yuen
Publisher:
ISBN:
Category : Iron-nickel alloys
Languages : en
Pages : 412

Get Book Here

Book Description


Modelling of Crack Growth in Single-Crystal Nickel-Base Superalloys

Modelling of Crack Growth in Single-Crystal Nickel-Base Superalloys PDF Author: Christian Busse
Publisher: Linköping University Electronic Press
ISBN: 9179299830
Category :
Languages : en
Pages : 55

Get Book Here

Book Description
This dissertation was produced at the Division of Solid Mechanics at Linköping University and is part of a research project, which comprises modelling, microstructure investigations and material testing of cast nickel-base superalloys. The main objective of this work was to deepen the understanding of the fracture behaviour of single-crystal nickel-base superalloys and to develop a model to predict the fatigue crack growth behaviour. Frequently, crack growth in these materials has been observed to follow one of two distinct cracking modes; Mode I like cracking perpendicular to the loading direction or crystallographic crack growth on the octahedral {111}-planes, where the latter is associated with an increased fatigue crack growth rate. Thus, it is of major importance to account for this behaviour in component life prediction. Consequently, a model for the prediction of the transition of cracking modes and the correct active crystallographic plane, i.e. the crack path, and the crystallographic crack growth rate has been developed. This model is based on the evaluation of appropriate crack driving forces using three-dimensional finite-element simulations. A special focus was given towards the influence of the crystallographic orientation on the fracture behaviour. Further, a model to incorporate residual stresses in the crack growth modelling is presented. All modelling work is calibrated and validated by experiments on different specimen geometries with different crystallographic orientations. This dissertation consists of two parts, where Part I gives an introduction and background to the field of research, while Part II consists of six appended papers. Die vorliegende Dissertation wurde in der Abteilung für Festigkeitslehre an der Universität von Linköping erstellt und ist Teil eines Forschungsprojektes, welches Modellierung, Mikrostrukturuntersuchungen und Materialtests von gegossenen nickelbasierten Superlegierungen umfasst. Das Hauptziel dieser Arbeit war es, das Verständnis des Bruchverhaltens von einkristallinen Superlegierungen auf Nickelbasis zu vertiefen und ein Modell zur Vorhersage des Wachstumsverhaltens von Ermüdungsrissen zu entwickeln. Es wurde beobachtet, dass das Risswachstum in diesen Materialien einem von zwei unterschiedlichen Rissmodi folgt; Modus I Rissfortschritt senkrecht zur Belastungsrichtung oder kristallographisches Risswachstum auf den oktaedrischen f111g-Ebenen, wobei letzteres mit einer erhöhten Ermüdungsrisswachstumsrate verbunden ist. Somit ist es von grosser Bedeutung dieses Verhalten in der Lebensdauervorhersage einer Komponente zu berücksichtigen. Demzufolge wurde ein Modell für die Vorhersage des Übergangs zwischen den Rissmodi und der korrekten aktiven kristallographischen Ebene, d.h. des Risspfades, sowie der kristallographischen Risswachstumsrate erarbeitet. Dieses Modell basiert auf geeigneten Rissantriebskräften, welche mit Hilfe dreidimensionaler Finite-Elemente-Simulationen berechnet werden. Im Fokus stand insbesondere der Einuss der kristallographischen Orientierung auf das Bruchverhalten. Ausserdem wird ein Modell zur Berücksichtigung von Restspannungen in der Risswachstumsmodellierung präsentiert. Alle Modellierungsarbeiten wurden durch Experimente an verschiedenen Probengeometrien mit unterschiedlichen kristallographischen Orientierungen kalibriert und validiert. Diese Dissertation besteht aus zwei Teilen, wobei Teil I aus einer Einführung und einem Hintergrund in das Forschungsgebiet und Teil II aus sechs beigefügten Forschungsartikeln besteht.

Short Fatigue Crack Growth in a Nickel-base Superalloy at Room and Elevated Temperature

Short Fatigue Crack Growth in a Nickel-base Superalloy at Room and Elevated Temperature PDF Author: J. C. Healy
Publisher:
ISBN:
Category : Materials
Languages : en
Pages :

Get Book Here

Book Description


The Effect of Elevated Temperature Pre-exposure on the Crack Growth Behaviour of a Polycrystalline Nickel-base Superalloy

The Effect of Elevated Temperature Pre-exposure on the Crack Growth Behaviour of a Polycrystalline Nickel-base Superalloy PDF Author: D. W. Hunt
Publisher:
ISBN:
Category : Materials
Languages : en
Pages :

Get Book Here

Book Description